NOVELTY - Rubber comprises 100 pts. wt. rubber, 30-80 pts. wt. carbon black, 1-8 pts. wt. zinc oxide, 0.5-4 pts. wt. stearic acid, 1-5 pts. wt. sulfur, 0.2-4 pts. wt. accelerator and 1-5 pts. wt. modified graphene, where the modified graphene is prepared by uniformly mixing graphite and modifier by ball milling, adding tert-butyl nitrite and solvent, ball milling, uniformly mixing, washing and drying, where the modifier comprises aminopropionanilide, 4-aminobenzanilide, 2-amino-N-cyclohexyl-N-methylbenzylamine, 4-(4-isopropylpiperazin-1-yl)aniline, (4-aminobenzene)-4-(4-methoxyphenyl)piperazine, (4-(4-aminobenzyl)piperazin-1-yl)ethanone and/or (4-aminobenzene)-4-(4-methoxyphenyl)piperazine. USE - Rubber used in synthetic rubber. ADVANTAGE - The rubber has excellent anti-aging effect.