▎ 摘 要
NOVELTY - Preapring graphene pitch-based active carbon involves adding asphalt, graphite and activator, mixing to obtain mixed material, subjecting mixed material under protection atmosphere, and activating for 3-10 hours at 400-650 degrees C to obtain graphene-pitch-based active carbon. USE - Method for preparing graphene pitch-based active carbon in super capacitor (claimed). ADVANTAGE - The method enables to preparing graphene pitch-based active carbon that is suitable for the mass production, does not need to add template agent, and in simple and cost effective manner. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a assembling super capacitor, which involves mixing graphene-pitch-based active carbon and binder to obtain mixed slurry, coating mixed slurry on conductive film, drying and cutting, assembling super capacitor.