▎ 摘 要
NOVELTY - A coating comprises 20-30 pts. wt. deionized water, 5-10 pts. wt. hydrogen peroxide, 5-10 pts. wt. activated carbon, 3-6 pts. wt. denatured alcohol, 3-5 pts. wt. graphene, 2-4 pts. wt. vinegar, 1-3 pts. wt. polyurethane, 0.5-1 pt. wt. epoxy resin and 1-3 pts. wt. modifier. The modifier comprises 1-2 pts. wt. lemon juice, 2-4 pts. wt. lemon peel, 2-4 pts. wt. orange peel, 1-3 pts. wt. Begonia extract, 1-3 pts. wt. Commelina, 1-2 pts. wt. seaweed, 0.6-1.2 pts. wt. calamine and 5-10 pts. wt. deionized water. USE - Coating for glass. ADVANTAGE - The formaldehyde-free coating has excellent adhesive property. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of coating.