▎ 摘 要
NOVELTY - Wear-resistant rubber-modified graphene comprises 48.9-56.5 wt.% synthetic rubber, 1.5-2.5 wt.% vulcanization accelerator, 8-18 wt.% graphene, 25-30 wt.% filler, 1.5-5 wt.% plasticizer and 0.1-3 wt.% additive. USE - Wear-resistant rubber-modified graphene. ADVANTAGE - The material has improved strength, heat resistance and frictional resistance.