• 专利标题:   Graphene solvent-free epoxy resin conductive floor coating primer comprises graphene-containing epoxy resin first component comprises low molecular weight epoxy resin and component containing alicyclic amine curing agent.
  • 专利号:   CN110408305-A
  • 发明人:   YANG J, SHEN X, WU J, SHI H, WU Y, YANG C
  • 专利权人:   JIANGSU SHANLI PAINT IND CO LTD
  • 国际专利分类:   C09D163/00, C09D005/08, C09D005/24
  • 专利详细信息:   CN110408305-A 05 Nov 2019 C09D-163/00 201990 Pages: 8 Chinese
  • 申请详细信息:   CN110408305-A CN10617830 10 Jul 2019
  • 优先权号:   CN10617830

▎ 摘  要

NOVELTY - Graphene solvent-free epoxy resin conductive floor coating primer comprises a graphene-containing epoxy resin first component having a mass ratio of 100:31 and a component containing an alicyclic amine curing agent. The graphene-containing epoxy resin first component comprises a low molecular weight 618 epoxy resin having an epoxy equivalent of 184-200, an SM60 trimethylolpropane polyglycidyl ether having an epoxy equivalent of 135-160, and an epoxy equivalent of 290-310 glycidyl ether, SM660A butyl glycidyl ether of epoxy equivalent of 140-167, S400 graphene, 912 dispersant, and 3,78 dispersant. The alicyclic amine-containing curing agent second component includes a YH505 alicyclic amine curing agent, a 1102 cardanol curing agent, and a DMP-30 curing accelerator. USE - Graphene solvent-free epoxy resin conductive floor coating primer. ADVANTAGE - The graphene solvent-free epoxy resin conductive floor coating primer is helps to utilizes the excellent static conductivity of graphene, and has excellent electrostatic conductivity, acid and alkali resistance, wear resistance and excellent mechanical properties, bonding strength of greater than or equal to 3 mega Pascal, and has a bonding strength greater than or equal to 5 mega Pascal. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a graphene solvent-free epoxy resin conductive floor paint primer, which involves: (A) preparing a graphene-containing epoxy resin first component finished product of 1.1, low molecular weight 618 epoxy resin, SM60 trimethylolpropane polyglycidyl ether, SM90 glycidyl ether and SM660A butyl glycidyl ether is uniformly mixed, adding graphene, 912 dispersant, 3,78 dispersant, stirring at high speed for 30 minutes to form a uniform viscous liquid, and the filter package is the finished product of graphene-containing epoxy resin first component; (B) preparing component containing the alicyclic amine curing agent of 2.1 by adding YH505 alicyclic amine curing agent, 1102 cardanol curing agent, DMP-30 curing accelerator into the mixing tank and mixing, and then filling the plastic in the barrel to obtain alicyclic amine curing agent component; and (C) adding the finished product of the alicyclic amine curing agent second component to the finished product of the graphene-containing epoxy resin first component, and mixing and putting it into use.