• 专利标题:   Organic-inorganic solid waste composite sound insulation material used in building applications, comprises organic solid waste particles, inorganic solid waste powder, light aggregate, water reducer, retarder, water, and nano aerogel containing nano silicon dioxide aerogel.
  • 专利号:   CN116082010-A
  • 发明人:   LI X, SHI B, WANG J, WU H, KANG S, YANG W, GAO Y, MA P, CHENG B
  • 专利权人:   CHINA WEST CONSTR GROUP CO LTD, CHINA WEST CONSTR BUILDING MATERIALS
  • 国际专利分类:   C04B111/20, C04B111/40, C04B111/52, C04B028/14, C04B038/08
  • 专利详细信息:   CN116082010-A 09 May 2023 C04B-028/14 202352 Chinese
  • 申请详细信息:   CN116082010-A CN11647068 21 Dec 2022
  • 优先权号:   CN11647068

▎ 摘  要

NOVELTY - An organic-inorganic solid waste composite sound insulation material comprises 15-40 pts. wt. organic solid waste particles moving in plasma atmosphere, 60-85 pts. wt. inorganic solid waste powder, 5-10 pts. wt. light aggregate, 0.2-1 pts. wt. water reducer, 0.06-0.12 pts. wt. retarder, 30-50 pts. wt. water, and 1-5 pts. wt. nano aerogel. When the organic solid waste particles move in the plasma atmosphere, the processing power is 60-500W, and the processing time is 5-300 seconds. The organic solid waste particle is 40-80 mesh waste rubber. The light aggregate is silver ion-containing graphene ceramic porcelain granule, and the silver ion and graphene are uniformly distributed on the surface and the inner portion of the ceramic porcelain granule. USE - Organic-inorganic solid waste composite sound insulation material used in building applications for producing cement, aggregate, brick, glass and ceramic building material. ADVANTAGE - The organic-inorganic solid waste composite sound insulation material has excellent sound absorption and sound insulation performance. DETAILED DESCRIPTION - An organic-inorganic solid waste composite sound insulation material comprises 15-40 pts. wt. organic solid waste particles moving in plasma atmosphere, 60-85 pts. wt. inorganic solid waste powder, 5-10 pts. wt. light aggregate, 0.2-1 pts. wt. water reducer, 0.06-0.12 pts. wt. retarder, 30-50 pts. wt. water, and 1-5 pts. wt. nano aerogel. When the organic solid waste particles move in the plasma atmosphere, the processing power is 60-500 W, and the processing time is 5-300 seconds. The organic solid waste particle is 40-80 mesh waste rubber. The light aggregate is silver ion-containing graphene ceramic porcelain granule, and the silver ion and graphene are uniformly distributed on the surface and the inner portion of the ceramic porcelain granule. The ceramic porcelain granule has grain diameter of 3-6 mm, porosity of 18% or more, adsorption rate of 20% or more, compression strength of 1 MPa or more, and spherical degree of 0.95 or more. The nano aerogel is nano carbon nano tube aerogel, nano silicon dioxide aerogel, nano aluminum oxide aerogel and/or nano titanium dioxide aerogel. An INDEPENDENT CLAIM is included for preparation of organic-inorganic solid waste composite sound insulation material.