▎ 摘 要
NOVELTY - A microwave-assisted Hemin-graphene/poly(3,4-ethylenedioxythiophene) ternary complex comprises 14-30 wt.% high iron chloride heme, 1-10 wt.% poly(3,4-ethylenedioxythiophene) and 60-84 wt.% reduced graphene oxide. USE - Microwave-assisted Hemin-graphene/poly(3,4-ethylenedioxythiophene) ternary complex. ADVANTAGE - The method is simple and low-cost. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of microwave-assisted Hemin-graphene/poly(3,4-ethylenedioxythiophene) ternary complex comprising taking high iron chloride heme, reduced graphene oxide and ammonium hydroxide, mixing, adding poly(3,4-ethylenedioxythiophene), stirring, microwave heating at 110-180 degrees C for 5-40 minutes, cooling, centrifuging, filtering, vacuum drying.