• 专利标题:   Four-element hybrid recognized nonyl phenol biomimetic composite material preparing method, involves coating graphene film on glassy carbon electrode surface, removing imprinted molecule, and carrying-out nonyl phenol preparing process.
  • 专利号:   CN103558283-A
  • 发明人:   WANG M, LI T, WANG S, WANG J, SHE Y
  • 专利权人:   INST QUALITY STANDARDS TESTING TECHNOL
  • 国际专利分类:   G01N027/48
  • 专利详细信息:   CN103558283-A 05 Feb 2014 G01N-027/48 201424 Pages: 9 Chinese
  • 申请详细信息:   CN103558283-A CN10581121 18 Nov 2013
  • 优先权号:   CN10581121

▎ 摘  要

NOVELTY - The method involves coating a graphene film on a glassy carbon electrode surface. Drying process is carried-out to obtain a GR/IL/GCE composite electrode. Chloroauric acid solution and sulfydryl aniline acetonitrile solution are poured into the GR/IL/GCE three-dimensional composite electrode. Control potential range is about -1.2-0.8 V. Scanning speed is about 50 mV/s to 100 mV/S. Phenol acetonitrile solution is kept for 2 hours. Concentration of tetrabutyl ammonium perchlorate is about 25 mmol/L. Imprinted molecule is removed. Nonyl phenol preparing process is carried-out. USE - Four-element hybrid recognized nonyl phenol biomimetic composite material preparing method. ADVANTAGE - The method enables shortening detection time, ensuring high selectivity effect and less detection limit, reducing cost and realizing detect nonyl molecule in a rapid manner. DESCRIPTION OF DRAWING(S) - The drawing shows a graphical view illustrating a four-element hybrid recognized nonyl phenol biomimetic composite material preparing method. '(Drawing includes non-English language text)'