• 专利标题:   Electrically conductive nylon composite material comprises polyamide, graphene, antioxidant, coupling agent, toughening agent, and silicone oil.
  • 专利号:   CN103740102-A, CN103740102-B
  • 发明人:   XU D, LUO Y
  • 专利权人:   ANHUI KEJU NEW MATERIAL CO LTD, ANHUI KEJU NEW MATERIAL CO LTD
  • 国际专利分类:   B29C047/92, C08K013/02, C08K003/04, C08K005/544, C08L051/06, C08L077/06, C08L083/04
  • 专利详细信息:   CN103740102-A 23 Apr 2014 C08L-077/06 201439 Pages: 7 Chinese
  • 申请详细信息:   CN103740102-A CN10745328 27 Dec 2013
  • 优先权号:   CN10745328

▎ 摘  要

NOVELTY - Electrically conductive nylon composite material comprises 82-90 wt.% of polyamide 1212, 1-5 wt.% of graphene, 0.1-1 wt.% of antioxidant, 0.5-1 wt.% of coupling agent, 8-13 wt.% of toughening agent, and 0.5-1 wt.% of silicone oil. USE - Electrically conductive nylon composite material. ADVANTAGE - The electrically conductive nylon composite material can be simply prepared with good toughness. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparing composite material comprising mixing the polyamide 1212 and silicon oil in a mixer for 3-7 minutes to obtain mixed materials and then adding into coupling agent, toughening agent, antioxidant and graphene to mix for 3-7 minutes, extruding the mixed raw material in a double-screw extruder at first section temperature of 180-220 degrees C, a second section temperature of 180-220 degrees C, a third section temperature of 180-220 degrees C, a fourth section temperature of 180-220 degrees C for 1-2 minutes and then melting and pelleting.