▎ 摘 要
NOVELTY - Graphene reinforced antistatic rubber composition comprises 75-100 pts. wt. rubber, 0.1-10 pts. wt. graphene, 1-20 pts. wt. carbon nanotubes, 1-25 pts. wt. flow modifiers, 0.1-10 pts. wt. antioxidant and 1-4 pts. wt. sulfur. USE - Used as graphene reinforced antistatic rubber composition. ADVANTAGE - The method improves dispersibility graphene, has reinforcing effect and avoids graphene agglomeration and low dispersion. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing graphene reinforced antistatic rubber composition comprising mixing, graphene, carbon nanotubes, rubber, antioxidants, flow modifier thoroughly mixed in mixing equipment, mixing at 70-200 degrees C, mixing time for 7-60 minutes to obtain pre-mixed masterbatch, removing sulfur, the vulcanization accelerator continues to be mixed with masterbatch in mixing equipment in proportion, where the temperature of the mixed rubber reaches 70-200 degrees C and discharging, plasticizing on a two-roll open mill and discharging tablets.