▎ 摘 要
NOVELTY - Preparing conductive ink formulation involves weighing 0.20-20 wt.% water-soluble polymer, 0.5-20 wt.% polyglycerol as the drying retarding agent, and amount less than 80% electrically conductive nanoparticles the carbon black (NF) and/or graphene (GF) and/or graphite (GR) and combinations. The amount of water sufficient to dissolve the water soluble polymer where amount of water is sufficient to make up the total weight of the formulation. USE - Method for preparing conductive ink formulation. ADVANTAGE - The method enables to prepare conductive ink formulation, which has great resistance to adhesion and abrasion, and environmentally friendly.