• 专利标题:   Radiation-proof clothes comprises inner layer, first layer, shielding layer, second layer, outer layer and antibacterial oil stain-resistant layer, first layer comprises e.g. graphene oxide, aluminum, carbonyl iron powder and bonding agent.
  • 专利号:   CN108198641-A
  • 发明人:   CHEN X
  • 专利权人:   SHENZHEN EVERYTHING IND CO LTD
  • 国际专利分类:   G21F001/12, C09D005/14, C09D005/16, C09D175/04, C09D007/61
  • 专利详细信息:   CN108198641-A 22 Jun 2018 G21F-001/12 201846 Pages: 7 Chinese
  • 申请详细信息:   CN108198641-A CN10026641 11 Jan 2018
  • 优先权号:   CN10026641

▎ 摘  要

NOVELTY - Radiation-proof clothes comprises inner layer, first layer, shielding layer, second layer, outer layer, and antibacterial oil stain-resistant layer from inside to the outside orderly, where the first layer comprises 2-20 pts. wt. graphene oxide, 50-90 pts. wt. aluminum, 50-90 pts. wt. carbonyl iron powder, 10-30 pts. wt. bonding agent, 1-5 pts. wt. flatting agent, 1-5 pts. wt. surfactant, second absorbing layer and the components of the first absorbing layer components are the same, the antibacterial oil stain-resistant layer comprises 5-30 pts. wt. inorganic silver antibacterial agent, 10-50 pts. wt. nano super-hydrophobic coating and 30-80 pts. wt. water. USE - Used as radiation-proof clothes. ADVANTAGE - The method: reduces secondary reflection, multiple reflection of electromagnetic waves, and number of cleanings; and increases number of repeated wears. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the clothes comprising (i) (a) ultrasonicizing the graphene oxide into a homogeneous solution in water, then adding to the uniformly stirred sendust and carbonyl iron powder aqueous solution, stirring, filtering, using hydrazine hydrate, washing for one time using water and ethanol, and drying to obtain wave absorber, (b) blending the wave absorber with the adhesive, adding auxiliary agent, and stirring for 2-6 hours to obtain absorbing coating, (ii) coating the absorbing coating on the inner side of the shielding layer, drying at 60-90 degrees C for 2-3 minutes, drying to obtain first layer, and (iii) (a) mixing the inorganic antibacterial agent, nanometer super-hydrophobic coating, blending water, stirring for 0.5-2 hours to obtain coating, and (b) the coating the coating on the outer layer, drying at 60-90 degrees C for 2-3 minutes, and drying to obtain antibacterial oil stain-resistant layer. DESCRIPTION OF DRAWING(S) - The drawing shows a schematic representation of the radiation-proof clothes.