▎ 摘 要
NOVELTY - A low temperature coating comprises 100 pts. wt. silicone emulsion, 5-15 pts. wt. acrylic emulsion, 60-75 pts. wt. dibutyl sebacate, 15-35 pts. wt. triethylhexyl phosphate, 1-5 pts. wt. graphene, 5-20 pts. wt. ethylene glycol, 1-8 pts. wt. glass fiber, 5-10 pts. wt. nano-zinc oxide gel solution, 6-10 pts. wt. dispersant, 5-10 pts. wt. leveling agent and 150-180 pts. wt. deionized water. USE - Low temperature coating. ADVANTAGE - The coating has reliable low temperature performance, has no foaming, cracking, shedding and discoloration. It is washable, durable, anticorrosive, moisture proof and has anti-dust functions. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of low temperature coating comprising taking 50% raw materials, adjusting pH value to 7.0-8.0, adding remaining raw materials, adjusting pH value to 8.0-8.5, and grinding for 10-30 minutes.