• 专利标题:   Antioxidant aqueous coating for artifact surface, comprises rutile titanium dioxide nanoparticles, graphene, sodium chloride, sodium borate, zinc oxide, bamboo charcoal fiber, vinegar, defoamers and water.
  • 专利号:   CN105694547-A
  • 发明人:   LI W, XU Q, LI S
  • 专利权人:   SUZHOU BEC BIOLOGICAL TECHNOLOGY CO LTD
  • 国际专利分类:   C09D001/00
  • 专利详细信息:   CN105694547-A 22 Jun 2016 C09D-001/00 201657 Pages: 5 Chinese
  • 申请详细信息:   CN105694547-A CN10104943 26 Feb 2016
  • 优先权号:   CN10104943

▎ 摘  要

NOVELTY - An antioxidant aqueous coating comprises 22-48 pts. wt. rutile titanium dioxide nanoparticles, 14-28 pts. wt. graphene, 15-30 pts. wt. sodium chloride, 9-22 pts. wt. sodium borate, 8-19 pts. wt. zinc oxide, 19-45 pts. wt. bamboo charcoal fiber, 13-28 pts. wt. vinegar, 7-12 pts. wt. defoamers and 35-60 pts. wt. water. USE - Antioxidant aqueous coating for artifact surface. ADVANTAGE - The antioxidant aqueous coating has excellent antioxidant properties and long aging properties. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of antioxidant aqueous coating, involves adding bamboo charcoal fiber in high temperature resistance furnace, carrying out radiant heating, maintaining temperature at 1200-1400 degrees C for 1-2 hours, lowering the firing temperature to 45-60 degrees C, grinding to obtain powder having size of 400-600 mesh, added vinegar with the powder, carrying out reaction, stirring for 0.5-1.2 hours, collecting the filtrate by filtration, then adding rutile titanium dioxide nanoparticles, graphene, sodium chloride, sodium borate, zinc oxide added to the filtrate, stirring at 56-78 degrees C for 1-2 hours, and then adding water and defoamer and stirring for 10-45 minutes.