• 专利标题:   Mesoporous molecular sieve-graphene flame-retardant plastic material for automobiles, contains comprises acrylonitrile-butadiene-styrene copolymer, linear phenolic resin, microencapsulated red phosphorus, and butyronitrile rubber.
  • 专利号:   CN106543631-A
  • 发明人:   QIANG J
  • 专利权人:   ANHUI BIG DIPPER SIGNAGE SYSTEM CO LTD
  • 国际专利分类:   C08K013/06, C08K003/04, C08K003/22, C08K003/32, C08K003/34, C08K007/08, C08K007/26, C08K009/10, C08L055/02, C08L061/06, C08L083/04, C08L009/02
  • 专利详细信息:   CN106543631-A 29 Mar 2017 C08L-055/02 201740 Pages: 5 Chinese
  • 申请详细信息:   CN106543631-A CN10937386 25 Oct 2016
  • 优先权号:   CN10937386

▎ 摘  要

NOVELTY - A mesoporous molecular sieve-graphene flame-retardant plastic material comprises acrylonitrile-butadiene-styrene copolymer, linear phenolic resin, microencapsulated red phosphorus, basic magnesium sulfate whisker, butyronitrile rubber, mesoporous molecular sieve SBA-15, ammonium polyphosphate, melamine formaldehyde resin, kaolin, antimony trioxide, dimethyl silicone oil, graphene, light calcium carbonate, potassium titanate whisker, liquid paraffin, superfine talc powder, ethanol, distilled water, and acetic acid. USE - Mesoporous molecular sieve-graphene flame-retardant plastic material is used for automobiles. ADVANTAGE - The mesoporous molecular sieve-graphene flame-retardant plastic material has excellent bonding property, thermal stability, and mechanical property. DETAILED DESCRIPTION - A mesoporous molecular sieve-graphene flame-retardant plastic material comprises 40-50 pts. wt. acrylonitrile-butadiene-styrene copolymer, 5-10 pts. wt. linear phenolic resin, 5-10 pts. wt. microencapsulated red phosphorus, 3-5 pts. wt. basic magnesium sulfate whisker, 2-5 pts. wt. butyronitrile rubber, 5-10 pts. wt. mesoporous molecular sieve SBA-15, 5-10 pts. wt. ammonium polyphosphate, 2-5 pts. wt. melamine formaldehyde resin, 2-3 pts. wt. kaolin, 5-8 pts. wt. antimony trioxide, 1-2 pts. wt. dimethyl silicone oil, 6-8 pts. wt. graphene, 5-10 pts. wt. light calcium carbonate, 2-5 pts. wt. potassium titanate whisker, 1-2 pts. wt. liquid paraffin, 3-5 pts. wt. superfine talc powder, ethanol, distilled water, and acetic acid. An INDEPENDENT CLAIM is included for preparation of plastic material.