▎ 摘 要
NOVELTY - A graphene heavy anticorrosive paint comprises component A and 10-40 pts. wt. curing agent component B. The component A comprises 100 pts. wt. matrix resin, 10-20 pts. wt. graphene, 5-15 pts. wt. nano yttrium aluminum garnet, 20-40 pts. wt. filler, 0.5-2 pts. wt. dispersant, 1-3 pts. wt. antisettling agent, 0.5-1 pt. wt. accelerant and 0.3-1.5 pts. wt. antifoaming agent. USE - Graphene heavy anticorrosive paint. ADVANTAGE - The coating has good corrosion resistance and weather resistance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of graphene heavy anticorrosive paint comprising taking dispersant, matrix resin, antisettling agent, accelerant and defoaming agent, stirring at rate of 1500 revolutions/minute (rpm) for 30 minutes, adjusting stirring speed to 500 rpm, adding graphene and nano yttrium aluminum garnet, stirring for 1 hour at rate of 2500 rpm, reducing stirring speed to 1000 rpm, adding filler, stirring for 30 minutes at rate of 1500 rpm, adding curing agent, and mixing.