▎ 摘 要
NOVELTY - A graphene oxide/titania with adsorption properties is prepared by taking graphene oxide, adding 50-100 pts. wt. of 2:1 volume ratio of ethanol and water mixed solution, preparing 0.05 mg/mL graphene oxide solution, ultrasonicating for 15-25 minutes, taking 1 pt. wt. titania and 10-20 pts. wt. aqueous solution, ultrasonicating for 10 minutes to obtain titania dispersion solution, adding 1 pt. wt. graphene oxide solution, ultrasonicating for 20-30 minutes, stirring for 1 hour, reacting for 2-4 hours at 100-120 degrees C, carrying out centrifugal separation, washing with ethanol and deionized water, taking product, and drying at 65-75 degrees C for 15-24 hours. USE - Method for preparing graphene oxide/titania with adsorption properties for preparing adsorbent material for adsorbing methylene blue dye in water body (claimed). ADVANTAGE - The method is simple.