NOVELTY - Preparation of organic silicone conducting resin comprises weighing 20-30 pts. wt. dimethyl silicone polymer, 0.5-1.5 pts. wt. graphene, 0.5-3 pts. wt. styrene-acrylonitrile resin, 20-30 pts. wt. styrene-butadiene rubber, 10-15 pts. wt. polyvinyl formal resin, 10-20 pts. wt. N,N-dimethylformamide, 3-4 pts. wt. urea resin, 5-9 pts. wt. copper and 1-3 pts. wt. tetrahydrophthalic anhydride, placing in mixer, and stirring at 70-80 degrees C for 10-20 minutes to obtain premix; and adding premix to extruder, and extruding at 120-130 revolutions/minute to obtain organic silicone conducting resin. USE - Method for preparing organic silicone conducting resin. ADVANTAGE - The resin has good heat resistance, physical strength, water resistance, moisture resistance, electrical properties, ductility and elasticity after curing.