▎ 摘 要
NOVELTY - Manufacture of lithium titanate electrode material involves mixing water, 3-5 %mass sucrose, 3-5 %mass Triton X-100 (RTM: Tert-octyl phenoxy polyethoxy ethanol), adding 3-5 %mass graphene, stirring to obtain slurry (A), grinding at 150-250 rpm for 60-300 minutes, adding lithium titanate in a weight ratio of 5.5:4.5-6:4 to obtain slurry (B) and drying. USE - Manufacture of lithium titanate electrode material (claimed). ADVANTAGE - The manufactured lithium titanate electrode material improves charging and discharging rate of lithium titanate battery by 1-5% and capacity of lithium titanate battery by 1-8%, and eliminates heating of battery during the charging and discharging of battery. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for the following: (1) lithium titanate electrode material manufactured by the method; (2) lithium titanate electrode slurry; and (3) preparation of lithium titanate electrode slurry.