▎ 摘 要
NOVELTY - An antistatic graphene two-component polyurethane wood paint comprises main agent, curing agent and diluent in mass ratio of 100:40-50:50-80. The main agent comprises 65-75 %mass coconut oleoresin, 8-15 %mass graphene powder, 15-25 %mass viscosity adjusting diluent, 0.1-0.3 %mass defoamer, 0.1-0.2 %mass leveling agent, 0.1-0.5 %mass anti-settling agent, and 0.5-1 %mass dispersing agent. The curing agent comprises 55.0-75.0 %mass hexamethylene diisocyanate (HDI) biuret curing agent and 25.0-35.0 %mass butyl acetate. The diluent comprises 60.0-70.0 %mass butyl acetate, 15.0-20.0 %mass ethyl acetate, and 15.0-25.0 %mass propylene glycol methyl ether acetate. USE - Antistatic graphene two-component polyurethane wood paint. ADVANTAGE - The antistatic wood paint provides coating film with excellent decoration and protection effect, and is easy to apply. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the antistatic graphene two-component polyurethane wood paint, which involves separately mixing raw materials of main agent, curing agent and diluents and stirring to obtain main agent, curing agent and diluent, and stirring main agent, curing agent and diluent.