▎ 摘 要
NOVELTY - Obtaining suspension or solid sample of graphene involves performing pyrolysis of polymer in absence of oxygen in a furnace at 400-1200 degrees C, and performing exfoliation of pyrolyzed product to obtain the desired product. USE - Method for obtaining suspension or solid sample of graphene (claimed).