▎ 摘 要
NOVELTY - The method involves adding and mixing 90-110 parts mass iron powder, 0.2-0.4 part mass toner, 0.1-0.2 part mass silicon powder, 1.7-1.9 parts mass chrome powder, 0.1-0.3 parts mass manganese powder, 0.01-0.2 part mass titanium powder, 0.01-0.2 part mass copper powder, 0.02-0.15 part mass molybdenum powder, 0.1-0.3 part mass nickel powder, 0.2-0.3 part mass vanadium powder, 0.01-0.1 part mass phosphorus powder, 0.1-0.2 part mass BORON powder, 0.1-0.3 part mass tungsten powder, 20-30 parts mass epoxy resin, 5-10 parts mass alumina, 3-6 parts mass carbon fiber, 2-4 parts mass graphene, 2-4 parts mass kaolin, 4-8 parts mass borax, 2-4 parts mass basalt fiber, 8-12 parts mass curing agent, 3-8 parts mass antifoaming agent, 10-20 parts mass stabilizer and 1-2 parts mass diluent. USE - Method for preparing front and rear axle of high-strength automobile. ADVANTAGE - The front and rear axle axles have higher hardness performance, corrosion resistance and toughness and the strength is higher, the probability of breaking the shaft is greatly reduced, and the safety factor is higher.