▎ 摘 要
NOVELTY - Vulcanizing graphene comprises (i) adding 50 mg graphene oxide into a conical flask, adding 40-300 ml mercaptan, stirring uniformly, and adding 20-70 mg thiourea, (ii) heating the mixed liquid to 35-50 degrees C and ultrasonic processing for 30-60 minutes, (iii) continuously heating to 80-150 degrees C and refluxing for 3-10 hours, (iv) cooling to room temperature and respectively washing using ultrapure water and anhydrous ethyl alcohol for 2-4 times, and (v) blast drying at 30-38 degrees C. USE - The method is useful for vulcanizing graphene (claimed).