• 专利标题:   Macromolecular far-infrared foaming material comprises e.g. natural rubber, polyolefin elastomer, ethylene propylene diene monomer, isoprene rubber, dicumyl peroxide, graphite, sodium nitrate, potassium permanganate and sulfuric acid.
  • 专利号:   CN113337017-A
  • 发明人:   DING T, DING D, DING Y
  • 专利权人:   FUJIAN WUCHIHENG TECHNOLOGY DEV CO LTD
  • 国际专利分类:   C08J009/08, C08K013/06, C08K003/04, C08K005/098, C08K005/14, C08K009/06, C08L023/08, C08L023/16, C08L007/00, C08L009/00
  • 专利详细信息:   CN113337017-A 03 Sep 2021 C08L-007/00 202187 Pages: 6 Chinese
  • 申请详细信息:   CN113337017-A CN10566959 24 May 2021
  • 优先权号:   CN10566959

▎ 摘  要

NOVELTY - Macromolecular far-infrared foaming material comprises 30-45 pts. wt. natural rubber, 5-9 pts. wt. polyolefin elastomer, 10-12 pts. wt. ethylene propylene diene monomer, 8-14 pts. wt. white carbon black, 3-6 pts. wt. isoprene rubber, 2-5 pts. wt. zinc stearate, 5-8 pts. wt. graphene oxide, 6-9 pts. wt. zinc oxide, 3-8 pts. wt. odorless cross-linking agent, 3-5 pts. wt. stearic acid, 4-7 pts. wt. foaming agent and 5-8 pts. wt. silane coupling agent. The graphene oxide is prepared by utilizing graphite, sodium nitrate, potassium permanganate and concentrated sulfuric acid. USE - Used as macromolecular far-infrared foaming material. ADVANTAGE - The graphene oxide has good dispersibility in the natural rubber, and can better improve the far-infrared light-emitting rate of the graphene.