▎ 摘 要
NOVELTY - An erosion-resistant anticorrosive composite crystal film is prepared by mixing 5-10 pts. wt. graphene modified polyphenylene oxide, 10-15 pts. wt. polysilicoboroxane, 5-10 pts. wt. ceramic micropowder, 3-5 pts. wt. glass fiber, 3-5 pts. wt. modified nano zinc oxide, 3-5 pts. wt. modified nano molybdenum disulfide, 35-40 pts. wt. epoxy resin, 5-25 pts. wt. solvent, 1-10 pts. wt. diluent, 10-20 pts. wt. curing agent and 1-3 pts. wt. additive. USE - Erosion-resistant and anticorrosive composite crystal film. ADVANTAGE - The composite crystal film the is added with graphene modified polyphenylene oxide micropowder which can reduce film porosity, and improve compactness, impact resistance and anti-peeling ability.