▎ 摘 要
NOVELTY - Ultrasonic dispersion of graphite oxide is performed in water to form graphene oxide suspension, the suspension is filtered and obtained graphene oxide is heated at 500-1000 degrees C under protective gas atmosphere for 0.5-1 hour to obtain graphene. The graphene is transferred to environment maintained at -250 degrees C to -50 degrees C for 0.4-1 hour, and the graphene is cooled and annealed at 200-300 degrees C for 5-12 hours. USE - Manufacture of graphene (claimed). ADVANTAGE - The graphene is manufactured with large specific surface area.