▎ 摘 要
NOVELTY - The preparation method of graphene transparent conductive film involves adding 5-10 pts. wt. graphene, 25-40 pts. wt. styrene-acrylic emulsion, 5-10 pts. wt. nano-silver powder and 45-55 pts. wt. deionized water to a centrifuge tube, uniformly mixing, ultrasonically vibrating the mixture for 15-25 minutes to obtain a coating solution and then drying using a glass plate with a thickness of 100-200 mu m, coating the mixture, and drying. USE - The method is useful for preparation of graphene transparent conductive film (claimed). ADVANTAGE - The method enables economical preparation of graphene transparent conductive film with high yield and excellent conductivity.