• 专利标题:   Modified lithium-nickel-cobalt manganite, comprises nickel cobalt lithium manganate, nano-graphene, microcrystalline silicon powder, nano-carbon particles, carbon fiber, boron iron, antimony oxide and de-ionized water.
  • 专利号:   CN106129398-A
  • 发明人:   CHEN X
  • 专利权人:   CHEN X
  • 国际专利分类:   H01M010/0525, H01M004/505, H01M004/525
  • 专利详细信息:   CN106129398-A 16 Nov 2016 H01M-004/505 201681 Pages: 4 Chinese
  • 申请详细信息:   CN106129398-A CN10736535 29 Aug 2016
  • 优先权号:   CN10736535

▎ 摘  要

NOVELTY - A modified lithium-nickel-cobalt manganate comprises nickel cobalt lithium manganate, nano-graphene, microcrystalline silicon powder, nano-carbon particles, carbon fiber, boron iron, antimony oxide, hexafluorophosphoricacid silver, copper tetrahydroxyisoflavone sodium, maleic anhydride grafted compatilizer, ethylenediamine tetraacetic acid, titanic acid ester coupling agent, modified copper powder, conductive copper powder, nano-aluminum powder and de-ionized water. USE - Modified lithium-nickel-cobalt manganite. ADVANTAGE - The modified lithium-nickel-cobalt manganate is prepared with better service life, better consistency and large capacity, in a cost-effective and eco-friendly manner. DETAILED DESCRIPTION - A modified lithium-nickel-cobalt manganate comprises 800-1000 pts. wt. nickel cobalt lithium manganate, 10-18 pts. wt. nano-graphene, 3-5 pts. wt. microcrystalline silicon powder, 5-8 pts. wt. nano-carbon particles, 5-6 pts. wt. carbon fiber, 2-5 pts. wt. boron iron, 4-5 pts. wt. antimony oxide, 3-5 pts. wt. hexafluorophosphoricacid silver, 2-4 pts. wt. copper tetrahydroxyisoflavone sodium, 2-4 pts. wt. maleic anhydride grafted compatilizer, 5-6 pts. wt. ethylenediamine tetraacetic acid, 4-5 pts. wt. titanic acid ester coupling agent, 5-6 pts. wt. modified copper powder, 4-5 pts. wt. conductive copper powder, 5-8 pts. wt. nano-aluminum powder and 10-25 pts. wt. de-ionized water.