▎ 摘 要
NOVELTY - Preparation of cobalt antimonide/redox graphene nanocomposite material involves heating and dissolving antimony trioxide and cobalt nitrate hexahydrate in an alcohol solvent, cooling obtained clear and transparent solution, adding a reducing agent to the cooled solution, stirring at room temperature for 1-5 hours, obtaining a black precursor, dissolving the black precursor in a graphene oxide aqueous dispersion, hydrothermally reacting at 120-180 degrees C for 8-12 hours, cooling the reaction solution to room temperature, washing obtained product, grinding, and drying. USE - Preparation of cobalt antimonide/redox graphene nanocomposite material used as anode material of lithium ion battery/sodium ion battery (claimed). ADVANTAGE - The method enables economical preparation of cobalt antimonide/redox graphene nanocomposite material with excellent recyclability, by simple process.