• 专利标题:   Preparing nano adsorbent for treating dye waste water, involves adding polyvinylpyrrolidone, graphene oxide and secondary water into container, stirring while adding ammonia water and hydrazine hydrate, and cooling to room temperature.
  • 专利号:   CN107138140-A
  • 发明人:   LIU Z, GUO Y, HAN L
  • 专利权人:   UNIV SHANXI
  • 国际专利分类:   B01J020/26, B01J020/28, B01J020/30, C02F001/28, C02F101/30
  • 专利详细信息:   CN107138140-A 08 Sep 2017 B01J-020/26 201772 Pages: 7 Chinese
  • 申请详细信息:   CN107138140-A CN10355563 19 May 2017
  • 优先权号:   CN10355563

▎ 摘  要

NOVELTY - Preparing nano adsorbent involves adding the polyvinylpyrrolidone (PVP), graphene oxide and secondary water into the container, stirring for 3-30 minutes while adding ammonia water and hydrazine hydrate, where mass ratio of graphene oxide, PVP, ammonia and hydrazine is 1:2.5-3.5:100-200:10-20:6500-8500. The obtained product is reacted at 40-80 degrees C for 2-5 hours and cooled to room temperature. The obtained product is stirred at speed of 11000-13000 revolution per minute for 15-30 minutes to obtain solid and washed with secondary water for two times. USE - Method for preparing nano adsorbent for treating dye waste water (claimed). ADVANTAGE - The method enables to prepare nano adsorbent in cost-effective manner, has high chemical stability, good adsorption and decolorization effect. DETAILED DESCRIPTION - Preparing nano adsorbent involves adding the polyvinylpyrrolidone (PVP), graphene oxide and secondary water into the container, stirring for 3-30 minutes while adding ammonia water and hydrazine hydrate, where mass ratio of graphene oxide, PVP, ammonia and hydrazine is 1:2.5-3.5:100-200:10-20:6500-8500. The obtained product is reacted at 40-80 degrees C for 2-5 hours and cooled to room temperature. The obtained product is stirred at speed of 11000-13000 revolution per minute for 15-30 minutes to obtain solid and washed with secondary water for two times. The secondary water is added to the obtained product to obtain PVP-graphene material suspension.