▎ 摘 要
NOVELTY - Thermally conductive film comprises 15-30 pts. wt. modified acrylic oligomer, 20-30 pts. wt. zinc oxide, 10-20 pts. wt. butyl rubber, 20-30 pts. wt. chloroprene rubber, 8-15 pts. wt. thermal conductivity filler, 4-9 pts. wt. halogen-free epoxy resin and 7-10 pts. wt. graphene boron nitride nanoplatelet. USE - Used as thermally conductive film. ADVANTAGE - The film: has good thermal conduction, strong bonding ability, wear resistance, high temperature resistance, good stability, non-toxic and is environmentally friendly. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing thermally conductive film, comprising taking raw materials, adding to the mixer for stirring, stirring for 60 plus minus 30 minutes, transferring stirred plastic material to a twin-roll molding machine for molding and curing for 3-8 minutes.