• 专利标题:   Molybdenum disulfide/reduced graphene oxide/nickel nanoparticle composite material used as hydrogen evolution reaction catalyst comprises molybdenum disulfide nanosheet dispersed on reduced graphene oxide, and nickel nanoparticles.
  • 专利号:   CN108607582-A
  • 发明人:   LIANG Z, LIU C, LI J, MA S
  • 专利权人:   UNIV WEIFANG, UNIV BEIJING NORMAL
  • 国际专利分类:   B01J027/051, B01J035/02, C25B001/04, C25B011/04
  • 专利详细信息:   CN108607582-A 02 Oct 2018 B01J-027/051 201877 Pages: 13 Chinese
  • 申请详细信息:   CN108607582-A CN10529922 29 May 2018
  • 优先权号:   CN10529922

▎ 摘  要

NOVELTY - Molybdenum disulfide/reduced graphene oxide/nickel nanoparticle composite material comprises molybdenum disulfide nanosheet dispersed on reduced graphene oxide as substrate, and nickel nanoparticles dispersed on reduced graphene oxide substrate and molybdenum disulfide nanosheet. USE - Molybdenum disulfide/reduced graphene oxide/nickel nanoparticle composite material used as hydrogen evolution reaction catalyst in alkaline electrolyte (claimed). ADVANTAGE - The molybdenum disulfide/reduced graphene oxide/nickel nanoparticle composite material has hydrogen evolution reaction catalytic activity in acidic electrolyte and alkaline electrolyte, better hydrogen evolution reaction catalytic activity in alkaline electrolyte, simple and easy preparation, and low cost and easy to obtain raw materials. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of molybdenum disulfide/reduced graphene oxide/nickel nanoparticle composite material comprising dispersing graphene oxide in water to obtain graphene oxide dispersion liquid, mixing molybdenum source, sulfur source and graphene oxide dispersion liquid to obtain first reaction mixture, hydrothermally reacting at 180-220 degrees C for 18-30 hours, separating, washing, obtaining molybdenum disulfide/reduced graphene oxide composite material, dispersing in organic solvent to obtain molybdenum disulfide/reduced graphene oxide composite material dispersion, adding nickel source and hydrazine hydrate into the molybdenum disulfide/reduced graphene oxide composite material dispersion, adjusting the pH at 8-10 to obtain second reaction mixture, reacting at 50-70 degrees C for 0.5-3 hours, separating and washing.