• 专利标题:   Graphene heat conductive coating comprises graphene, nano carbon material, lauryl betaine, N-methylpyrrolidone, aqueous polyurethane, propylene glycol alginate, sodium sulfate and water.
  • 专利号:   CN110157310-A
  • 发明人:   TANG H, CHEN Z, LIN J, HU J, LI G, GUO X, LUO H, LAI H
  • 专利权人:   GUANGDONG HUALAN AUTO MATERIAL RES INST, QINGYUAN MINGYU MATERIAL TECHNOLOGY CO
  • 国际专利分类:   C09D175/04, C09D007/61
  • 专利详细信息:   CN110157310-A 23 Aug 2019 C09D-175/04 201972 Pages: 6 Chinese
  • 申请详细信息:   CN110157310-A CN10319031 11 Apr 2018
  • 优先权号:   CN10319031

▎ 摘  要

NOVELTY - Graphene heat conductive coating comprises 13-17 pts. wt. graphene, 4-9 pts. wt. nano carbon material, 14-20 pts. wt. lauryl betaine, 25-30 pts. wt. N-methylpyrrolidone, 40-60 pts. wt. aqueous polyurethane, 5-10 pts. wt. propylene glycol alginate, 2-5 pts. wt. sodium sulfate and 50-100 pts. wt. water. USE - Used as graphene heat conductive coating. ADVANTAGE - The coating has excellent thermal conductivity, heat resistance and adhesion. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing graphene heat conductive coating, comprising (i) mixing graphene, nano carbon material and water, and magnetically stirring for 10-20 minutes to obtain suspension, (ii) adding lauryl betaine and N-methylpyrrolidone into the suspension, adjusting the pH to 6-8, and magnetically stirring for 20-40 minutes, (iii) adding aqueous polyurethane and sodium sulfate into obtained suspension, magnetically stirring for 10-20 minutes, then adding propylene glycol alginate, magnetically stirring for 10-20 minutes, dispersing for 20-40 minutes in a high speed shear disperser, and ultrasonically dispersing for 10-20 minutes to obtain final product.