▎ 摘 要
NOVELTY - A silicone rubber contains 100 pts. wt. methyl vinyl silicone rubber, 1-10 pts. wt. carbon nanotube, 1-5 pts. wt. graphene, 0.5-3 pts. wt. vinyltrimethoxysilane and 0.5-3 pts. wt. hydroxy silicone oil. USE - Silicone rubber (claimed). ADVANTAGE - The silicone rubber has excellent conductivity, physical properties, mechanical properties and low density. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of silicone rubber, which involves weighing raw materials and then mixing, kneading the mixture and then heating at 140-160 degrees C for 1-2 hours, and cooling.