▎ 摘 要
NOVELTY - Producing biocompatible silver-graphene oxide polymer involves reacting 10 wt.% water, 84.10 wt.% propan-1,2,3-triol, 0.50 wt.% silver nanoparticles, 0.20 wt.% benzyl-dimethyl-tridecyl-azanium chloride, 0.20 wt.% tris (4-(dimethylamino) phenyl) methyl chloride, 2 wt.% 2-hydroxypropane-l,2,3-tricarboxylic acid and 3 wt.% oxide of graphene to obtain silver-graphene oxide polymer. USE - Method for producing biocompatible silver-graphene oxide polymer.