• 专利标题:   Adsorption film contains tourmaline powder, schweizerite powder, N-cyclohexyl-2-benzothiazole sulfenamide, activated carbon composite nano fiber, common Andrographis herb lactone, graphene, chloroparaffin, carboxylic acid, and flexibilizer.
  • 专利号:   CN107815128-A
  • 发明人:   ZHANG Y
  • 专利权人:   ZHANG Y
  • 国际专利分类:   C08J005/18, C08K013/02, C08K003/04, C08K003/34, C08K003/38, C08K005/09, C08L089/00, C08L091/06
  • 专利详细信息:   CN107815128-A 20 Mar 2018 C08L-091/06 201825 Pages: 4 Chinese
  • 申请详细信息:   CN107815128-A CN11085490 07 Nov 2017
  • 优先权号:   CN11085490

▎ 摘  要

NOVELTY - An adsorption film comprises 8-12 parts mass tourmaline powder, 8-12 parts mass schweizerite powder, 4-8 parts mass N-cyclohexyl-2-benzothiazole sulfenamide, 15-22 parts mass activated carbon composite nano fiber, 3-6 parts mass common Andrographis herb lactone, 8-18 parts mass graphene, 15-22 parts mass chloroparaffin, 4-12 parts mass carboxylic acid, 5-9 parts mass soybean peptide, and 7-10 parts mass flexibilizer. The flexibilizer is prepared by mixing sodium succinate, nano titania, triethanolamine, guar gum ether, and bamboo carbon fiber. USE - Adsorption film. ADVANTAGE - The adsorption film has excellent oxidation resistance, and mildew resistance even in oxygen-rich and humid environment, and is environmentally-friendly. DETAILED DESCRIPTION - An adsorption film comprises 8-12 parts mass tourmaline powder, 8-12 parts mass schweizerite powder, 4-8 parts mass N-cyclohexyl-2-benzothiazole sulfenamide, 15-22 parts mass activated carbon composite nano fiber, 3-6 parts mass common Andrographis herb lactone, 8-18 parts mass graphene, 15-22 parts mass chloroparaffin, 4-12 parts mass carboxylic acid, 5-9 parts mass soybean peptide, and 7-10 parts mass flexibilizer. The flexibilizer is prepared by mixing 0.9 pt. wt. sodium succinate, 6.3 pts. wt. nano titania, 0.5 pt. wt. triethanolamine, 0.1 pt. wt. guar gum ether, and 0.1 pt. wt. bamboo carbon fiber. An INDEPENDENT CLAIM is included for preparation of adsorption film, which involves mixing all components at 530 degrees C and 4.3 MPa, drying and crushing into a powder of 104 microns, coating the powder in a mold, and pressing.