• 专利标题:   Preparing osmosis film useful for desalinating, comprises dissolving high molecular polymer ethylenediamine in de-ionized water, adding amino graphene quantum point nano grains, stirring, soaking interfacial polymerization and drying.
  • 专利号:   CN107349787-A
  • 发明人:   SU B, ZHAO K, LI S
  • 专利权人:   UNIV CHINA OCEAN
  • 国际专利分类:   B01D061/00, B01D067/00, B01D069/12, B01D071/42, B01D071/60, C02F001/44, C02F103/08
  • 专利详细信息:   CN107349787-A 17 Nov 2017 B01D-061/00 201803 Pages: 8 Chinese
  • 申请详细信息:   CN107349787-A CN10576365 14 Jul 2017
  • 优先权号:   CN10576365

▎ 摘  要

NOVELTY - Preparing forward osmosis film comprises adding aminated graphene quantum dot aqueous solution to polyethyleneimine, the oil phase is benzene triformyl chloride solution, the steps includes (i) dissolving high molecular polymer ethylenediamine in de-ionized water, adding amino graphene quantum point nano grains, stirring uniformly, preparing into aqueous phase monomer solution, (ii) dissolving polybasic acyl chloride in organic solvent to obtain organic phase solution, (iii) soaking interfacial polymerization, reacting in aqueous phase monomer solution for 5-30 minutes, taking out and drying. USE - The osmosis film is useful for desalinating, sewage treating and/or food processing (claimed). ADVANTAGE - The method is simple and economical. DETAILED DESCRIPTION - Preparing forward osmosis film comprises adding aminated graphene quantum dot aqueous solution to polyethyleneimine, the oil phase is benzene triformyl chloride solution, the steps includes (i) dissolving high molecular polymer ethylenediamine in de-ionized water, adding amino graphene quantum point nano grains, stirring uniformly, preparing into aqueous phase monomer solution, (ii) dissolving polybasic acyl chloride in organic solvent to obtain organic phase solution, (iii) soaking interfacial polymerization, reacting in aqueous phase monomer solution for 5-30 minutes, taking out, drying film surface in air with aqueous phase monomer solution for 10-120 seconds to form complex layer, treating film interfacial polymerization at 50-80 degrees C for 5-30 minutes, removing the organic solvent and promoting interfacial polymerization.