• 专利标题:   Conductive material used for preparation of conductive electrode for soil electrokinetic remediation includes resin masterbatch, modified carbon fiber, modified graphene, modified alumina, coupling agent, dispersant, and antioxidant.
  • 专利号:   CN106336630-A, CN106336630-B
  • 发明人:   FU R
  • 专利权人:   FU R, FU R
  • 国际专利分类:   B09C001/06, C08K013/06, C08K003/04, C08K003/08, C08K003/22, C08K007/06, C08K009/02, C08K009/06, C08K009/08, C08L033/20, C08L067/02, C08L081/02, H01B001/24
  • 专利详细信息:   CN106336630-A 18 Jan 2017 C08L-067/02 201719 Pages: 19 Chinese
  • 申请详细信息:   CN106336630-A CN10756397 29 Aug 2016
  • 优先权号:   CN10756397

▎ 摘  要

NOVELTY - A conductive material comprises resin masterbatch, modified carbon fiber, modified graphene, modified alumina, coupling agent, dispersant, enhancer, ethoxylated trimethylolpropane triacrylate, antioxidant, dibutyl phthalate, and nano-copper powder. USE - Conductive material used for preparation of conductive electrode for soil electrokinetic remediation (all claimed). ADVANTAGE - The conductive material has excellent properties, and good scientific research and production value. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of conductive material comprising adding high-speed mixer with acrylonitrile-styrene-acrylate terpolymer, polybutylene terephthalate and polyphenylene sulfide, mixing at 100-120 degrees C to obtain resin masterbatch, adding 80-90% of modified carbon fiber, modified alumina, 70-80% of coupling agent, dispersant, ethoxylated trimethylolpropane triacrylate and nano-copper powder, mixing at 1300-1500 revolutions/minute for 10-20 minutes, feeding to double-screw extruder, and extruding at 130-140 degrees C; and adding remaining dosage of modified graphene and coupling agent, and remaining raw materials, and mixing for 20-30 minutes.