• 专利标题:   Eco-friendly adhesive protection gluing agent for compound backing plate of circuit board, comprises epoxy resin, chloroprene rubber, modified filler, coupling agent, solvent, curing agent, chlorinated graphene, water glass, polyvinyl alcohol, antioxidant and inorganic powder.
  • 专利号:   CN115029091-A
  • 发明人:   ZHONG L, LI R
  • 专利权人:   DONGGUAN XIANGHUA ELECTRONIC TECHNOLOGY
  • 国际专利分类:   C09J011/00, C09J011/04, C09J011/06, C09J011/08, C09J111/00, C09J163/00, C09J179/08
  • 专利详细信息:   CN115029091-A 09 Sep 2022 C09J-163/00 202296 Chinese
  • 申请详细信息:   CN115029091-A CN10810369 11 Jul 2022
  • 优先权号:   CN10810369

▎ 摘  要

NOVELTY - Eco-friendly adhesive protection gluing agent comprises 20-30 pts. wt. epoxy resin, 20-30 pts. wt. chloroprene rubber, 4-8 pts. wt. modified filler, 1-5 pts. wt. coupling agent, 30-60 pts. wt. solvent, 1-5 pts. wt. curing agent, 6-14 pts. wt. chlorinated graphene, 10-20 pts. wt. water glass, 1-5 pts. wt. polyvinyl alcohol, 0.1-3 pts. wt. antioxidant and 1-5 pts. wt. inorganic powder. USE - Eco-friendly adhesive protection gluing agent for compound backing plate of circuit board. ADVANTAGE - The eco-friendly adhesive has high in strength, and improves curing speed. The colloid has good thermal stability, high temperature resistance and insulating property. The preparation method of the eco-friendly adhesive is simple, and provides convenient operation and control. The produced product has high quality and cost-effective, and facilitates industrial production. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing eco-friendly adhesive, which involves: refining the toughening agent, adding the epoxy resin and the chloroprene rubber into the solvent, stirring uniformly, adding the refined toughening agent, and continuously stirring and mixing for 15-25 minutes to obtain a mixture A; mixing and heating chlorinated graphene, water glass, polyvinyl alcohol, inorganic powder and thermoplastic polyimide at 40-60℃, and continuously stirring for 15-25 minutes to obtain a mixture B; adding the modified filler, the coupling agent, the curing agent, the antioxidant and the mixture B into the mixture A, and stirring for 3-5 hours.