▎ 摘 要
NOVELTY - High molecular reflective coating comprises 0.5-0.8 pts. wt. modified graphene, 20-30 pts. wt. epoxy resin, 3-5 pts. wt. polydimethylsiloxane, 10-30 pts. wt. titanium pigment, 15-18 pts. wt. xylene-type fluorosilicone resin, 10-15 pts. wt. glass reflective micro-bead, 7-15 pts. wt. polyethylene silicone resin, 3-8 pts. wt. acrylic emulsion, 0.2-0.5 pts. wt. plasticizer, 0.5-1 pts. wt. flatting agent, 0.1-0.5 pts. wt. antifoaming agent, 0.5-1 pts. wt. dispersant, 20-30 pts. wt. water and hexamethylcyclotrisiloxane (balance amount). USE - The coating is useful in the construction field (claimed). ADVANTAGE - The coating has excellent reflective effect and high thermal conductivity. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing coating comprising (a) adding modified graphene, titanium dioxide and dispersant into water, and ultrasonically dispersing, (b) combining epoxy resin, polydimethylsiloxane, xylene type fluorosilicone resin, polyethyl silicone resin, hexamethylcyclotrisiloxane, acrylic emulsion, plasticizer, flatting agent and antifoaming agent and then mixing uniformly, and (c) mixing the mixture obtained in step (a) and (b), and adding glass reflective micro-bead.