▎ 摘 要
NOVELTY - Aqueous coating comprises 45-55 wt.% of aqueous resin, 5-15 wt.% of latent solvent, 10-20 wt.% of water, 5-25 wt.% of filler, and 5-10 wt.% of pigment. The filler is mixed powder of graphene microchip, carbide and nitride in a ratio of 6:1:3. The graphene microchip is obtained by wet grinding the graphene honeycomb crystal having specified thickness. USE - Aqueous coating. ADVANTAGE - The aqueous coating is cost-effective and eco-friendly, and has good radiating effect and excellent dispersibility and static spraying and flatting effects. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparing the aqueous coating comprising mixing aqueous resin and latent, then heating in water, softening the aqueous resin with water and latent solvent, uniformly stirring, then adding mixed material, pigment and filler, ball grinding the material for 4 hours using a ball mill and then diluting for 10 plus minus 1 seconds and packaging.