▎ 摘 要
NOVELTY - Aromatic alcohol oxidation method for preparing aldehyde, involves placing graphene-supported nano-copper powder and tetramethylpiperidine nitrogen oxide in a reaction apparatus, adding distilled water and aromatic alcohol and carrying out oxidation under oxygen at 80-140 degrees C for 4-8 hours. USE - Aromatic alcohol oxidation method for preparing aldehyde using graphene-supported nano-copper powder. ADVANTAGE - The conversion of aromatic alcohol is more than 96%, and the selectivity of aldehyde is more than 95%, and the catalytic performance is excellent.