▎ 摘 要
NOVELTY - The method involves performing high elastic polyester fiber ventilating process. Side seat height needle smelting face material cold pressing operation is carried out for 2-3 minutes. A non-steel ring cup is filled with 5-10 wt.pts of warm water and 2.5-5.0 wt.pts of graphite. Hot dissolving silicon glue is mixed with graphite alkene glue. Glue mixture is coated on a graphene film. A low-voltage power source is covered by the graphene film by a heating lead. A shoulder hook is connected to a decoration component for sewing the graphene film. USE - Movable graphite alkene heating film physical therapy bra manufacturing method. ADVANTAGE - The method enables manufacturing movable graphite alkene heating film physical therapy bra in a simple manner, and with better smoothing effect and better female breast safety. DESCRIPTION OF DRAWING(S) - The drawing shows a front view of a movable graphite alkene heating film physical therapy bra. '(Drawing includes non-English language text)'