▎ 摘 要
NOVELTY - A graphene-modified polypropylene material comprises 50-68 wt.% synthetic resin, 15-20 wt.% plasticizer, 1-5 wt.% stabilizer, 1-5 wt.% lubricant, 5-10 wt.% colorant, 5-12 wt.% graphene and 1-5 wt.% modified additive. USE - Graphene-modified polypropylene material (claimed). ADVANTAGE - The graphene-modified polypropylene material has excellent toughness, corrosion resistance, strength, lubricating effect and heat resistance.