▎ 摘 要
NOVELTY - Concrete appearance quality modifier attached to oily mold release agent is claimed. The concrete appearance quality modifier is prepared by ultrasonically dispersing organosilicon monomer solution, nano-paraffin emulsion, nano-graphene oxide, and modified nano-paraffin emulsion uniformly, where the organosilicon monomer solution is prepared by mixing organosilicon monomer and ethanol, and the modified nano-paraffin emulsion is prepared by mixing nano-paraffin emulsion, nano-graphite particles, nano-silicon dioxide, disodium edetate and calcium formate uniformly through ultrasonic dispersion. The concrete appearance quality modifier comprises 20-25 pts. wt. organosilicon monomer, 50 pts. wt. ethanol, 3-5 pts. wt. nano-graphene oxide, 80-90 pts. wt. nano-paraffin emulsion, 10-20 pts. wt. nano-graphite particles, 5-10 pts. wt. nano-silicon dioxide, 3-5 pts. wt. disodium edetate, and 5-10 pts. wt. calcium formate. USE - Used as a concrete appearance quality modifier attached to oily release agent. ADVANTAGE - The modifier promotes the elimination of air bubbles on the surface of the concrete, stabilizes the separation of water and oil phases, improves the surface quality of concrete and facilitates demolding. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are also included for: Preparing concrete appearance quality modifier attached to oily mold release agent; and Use method of concrete appearance quality modifier attached to oily mold release agent.