▎ 摘 要
NOVELTY - Nanocarboxylated graphene composite polyester conductive fabric preparation involves dissolving phenol in ethanol, and then dispersing nano-carboxylated graphene in an ethanol-phenol mixed solution under ultrasonic conditions to obtain black dispersion solution. The polyester fabric is dipped into the obtained solution at 40-60 degrees C for 5-30 minutes. The obtained nano-carboxylated graphene conductive polyester fabric is washed with ethanol, and then dried at 80 degrees C to get the nano-carboxylated graphene conductive polyester fabric. USE - Method for preparing nanocarboxylated graphene composite polyester conductive fabric (claimed). ADVANTAGE - The method prepares the nanocarboxylated graphene composite polyester conductive fabric in a simple and cost-effective manner with good conductivity.