▎ 摘 要
NOVELTY - Preparing oriented graphite material comprises mixing 12-22 wt.% intermediate phase asphalt, 4-5.5 wt.% thermoplastic resin and 72-82 wt.% natural graphite, stirring, cooling to 100-150 degrees C, adding 0.5-2 wt.% graphene oxide, stirring, cooling to room temperature, crushing into mixed powder, hot molding, and sintering in high temperature graphitizing furnace. USE - The method is useful for preparing oriented graphite material. ADVANTAGE - The method: increases the molecular interface bonding force; improves the strength and heat conducting performance of the material. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for graphite material prepared by above mentioned method.