• 专利标题:   Graphene oxide hollow brick comprises magnesium oxide, magnesium chloride, water, coal slag, nickel-chromium-iron alloy slag, graphene oxide, foaming agent, and concrete containing construction waste, magnesium oxide, water and acetic acid.
  • 专利号:   CN108164286-A
  • 发明人:   LI Z, LI W
  • 专利权人:   WEIHAI NANHAI CARBON MATERIALS TECHNOLOGY RES INST CO LTD
  • 国际专利分类:   C04B038/10, C04B028/32
  • 专利详细信息:   CN108164286-A 15 Jun 2018 C04B-038/10 201849 Pages: 9 Chinese
  • 申请详细信息:   CN108164286-A CN10161786 27 Feb 2018
  • 优先权号:   CN10161786

▎ 摘  要

NOVELTY - A graphene oxide hollow brick comprises 60-80 pts. wt., preferably 70 pts. wt. magnesium oxide, 16-20 pts. wt., preferably 18 pts. wt. magnesium chloride, 60-100 pts. wt., preferably 80 pts. wt. water, 10-30 pts. wt., preferably 20 pts. wt. coal slag, 40-60 pts. wt., preferably 50 pts. wt. nickel-chromium-iron alloy slag, 4-8 pts. wt., preferably 6 pts. wt. graphene oxide, 0.8-1.2 pts. wt., preferably 1 pt. wt. foaming agent, and 10-15 pts. wt., preferably 12 pts. wt. concrete. The concrete comprises 20-25 pts. wt. construction waste, 1-2 pts. wt. magnesium oxide, 5-8 pts. wt. aluminum sulfate slag, 1-1.5 pts. wt. ore tailings, 1.5-2 pts. wt. slag ash, 5-6 pts. wt. reed stalk powder, 5-6 pts. wt. sawdust wood chips, 0.5-1.5 pts. wt. rosin saponified ester, 5-8 pts. wt. acetic acid, 30-60 pts. wt. water, 0.5-1 pt. wt. waste aluminum powder, and nano silica hydrocolloid. USE - Graphene oxide hollow brick. ADVANTAGE - The graphene oxide hollow brick has excellent pressure resistance and earthquake resistance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the graphite oxide hollow brick, which involves using hydrogen-argon gas mixture.