▎ 摘 要
NOVELTY - The method involves dispersing graphene oxide powder in de-ionized water with mass concentration of 0.1 to 0.4 mg/mL. The graphene oxide powder is added with ammonia and water to gather dopamine. 10 to 30 g/L of dopamine is deposited on surface of a silver nitrate plating solution, where 10 to 60 g/L of glucose solution is added with the silver nitrate plating solution. A uniform and dense silver thin layer is coated on surface of a graphene oxide nano-layer with a high shape factor by heat treatment process. USE - Method for preparing highly conductive oxidized graphite alkene. ADVANTAGE - The method enables preparing highly conductive oxidized graphite alkene with short time, strong controllability and high conductivity. The prepared composite material has better coating performance and high bonding strength between the silver layer and the graphene oxide. DESCRIPTION OF DRAWING(S) - The drawing shows a screen shot illustrating a method for preparing highly conductive oxidized graphite alkene.