▎ 摘 要
NOVELTY - Preparation of graphene oxide/silver nanocomposite hybrid antibacterial material involves adjusting the pH of the graphene oxide aqueous solution to alkaline with a strong alkali solution, adding epichlorohydrin to alkaline graphene oxide aqueous solution, stirring and reacting at 50-70 degrees C for 2-5 hours, after cooling, using deionized water for centrifugal washing 3-5 times to obtain epichlorohydrin-modified graphene oxide, dispersing epichlorohydrin-modified graphene oxide in the carbonate buffer solution at a concentration of 0.3-3 g/l, mixing the amino-terminated hyperbranched polymer solution with the silver nitrate solution and heating it to boiling for 3-5 minutes, adding the amino-terminated hyperbranched polymer nano-silver solution to the epichlorohydrin modified graphene oxide solution, stirring, and reacting at 50-70 degrees C for 2-5 hours. USE - Preparation of graphene oxide/silver nanocomposite hybrid antibacterial material used for functionalizing fiber or fabric product (claimed). ADVANTAGE - The method is simple, and enables preparation of graphene oxide/silver nanocomposite hybrid antibacterial material. The prepared graphene oxide/silver nanocomposite hybrid antibacterial material provides functionalized fiber or fabric product with excellent antibacterial effect and antiviral effect. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for the following: (1) graphene oxide/silver nanocomposite hybrid antibacterial material, which is prepared by the method; (2) use of the graphene oxide/silver nanocomposite hybrid antibacterial material in the fiber/fabric which is subjected to padding assembly finishing in a finishing solution obtained from the graphene oxide/silver nanocomposite hybrid antibacterial material; and (3) fiber or fabric product, which comprises graphene oxide/silver nanocomposite hybrid antibacterial material.